title: "Chinese Scientists Create 10 µm Lithium Anodes: 504 Wh/kg Energy Density in Lab Tests"
description: "Chinese scientists from Shenzhen used screen printing to create lithium anodes starting from 10 µm thick. In lab tests, a configuration with a nickel-containing cathode showed a calculated energy density of 504 Wh/kg and stability over 260 cycles."
date: 2026-11-18T01:41:01.866Z
lang: en
url: https://xab.info/en/posts/china-lithium-anodes-10-um-energy-density-504-wh-kg
tags: [lithium-battery, solid-state-battery, ev-battery, china-science, energy-density, anode-technology]
author: "Alexander Buran"
publisher: "XAB.info"
---

# Chinese Scientists Create 10 µm Lithium Anodes: 504 Wh/kg Energy Density in Lab Tests

![Samples of ultrathin solid-state lithium batteries with 504 Wh/kg energy density on a laboratory table](https://xab.info/media/2026/11/18/kitaj-litievyje-anody-10-mkm-plotnost-energii-504-vt-ch-kg/kitaj-litievyje-anody-10-mkm-plotnost-energii-504-vt-ch-kg-1.webp)

## Key Points

- The Shenzhen team (CAS) developed a screen-printing method to create lithium anodes 10, 20, and 28 µm thick
- Adding a magnesium compound to molten lithium forms a protective layer that suppresses dendrite growth
- 10 µm anodes endured over 260 cycles with coulombic efficiency above 99.8%
- The configuration with a nickel-containing cathode and 20 µm anode achieved a calculated energy density of 504 Wh/kg and 1071 Wh/L
- Results are laboratory-scale; industrial scaling has not yet been performed

A research team from the Shenzhen Institutes of Advanced Technology under the Chinese Academy of Sciences, in cooperation with several academic institutions, has presented the results of developing ultrathin lithium anodes for rechargeable batteries. The key innovation lies in applying a screen-printing method, which produced anodes with equivalent thicknesses of 10, 20, and 28 micrometers. In one of the experimental configurations—featuring a nickel-containing cathode and a 20-micrometer anode—the calculated energy density reached 504 Wh/kg and 1071 Wh/L, significantly exceeding the metrics of most commercial lithium-ion batteries used in electric vehicles today.

### Screen Printing Instead of Deposition: How the Anode is Formed

The technological approach used by the researchers differs fundamentally from traditional methods of forming lithium anodes. Molten lithium is applied onto a copper substrate through a special screen mask, resulting in the formation of uniform microdisks on the surface. This approach ensures controlled lithium distribution across the anode area and allows precise specification of the layer thickness. According to the publication, experiments yielded three anode variants—10, 20, and 28 micrometers in equivalent thickness, opening up the possibility of matching configurations to specific battery weight and capacity requirements.

### Dendrites and the Role of Magnesium in the Protective Layer

One of the fundamental problems of metallic lithium as an anode material remains the formation of dendrites—thin needle-like crystalline structures that grow during cycling and can cause internal short circuits, capacity degradation, and fire hazards. To suppress this effect, researchers added a magnesium compound to the molten lithium. According to experimental results, magnesium promoted the formation of a protective layer on the anode surface, reducing the intensity of unwanted side chemical reactions and decreasing irreversible lithium losses during each charge-discharge cycle.

### Laboratory Test Results: 260 Cycles and Over 99.8% Efficiency

During laboratory tests, batteries equipped with anodes just 10 micrometers thick demonstrated stable operation for over 260 charge-discharge cycles with a coulombic efficiency exceeding 99.8%. This metric indicates that active lithium losses per cycle are extremely small, and capacity degradation within the tested range remains within acceptable limits. In the configuration with a nickel-containing cathode and a 20-micrometer anode, the calculated specific energy density was 504 Wh/kg, and the volumetric density was 1071 Wh/L. The researchers also tested the developed technology in batteries with a gel electrolyte, expanding the range of potential design solutions.

### From Lab to Production: Prospects and Limitations

At the current stage, all obtained results are laboratory-based and do not reflect industrial serial production conditions. Transitioning from experimental prototypes to mass production will require solving challenges in scaling up screen printing, ensuring parameter stability over large anode areas, and integrating the technology into existing production lines. Nevertheless, according to the authors, the method is potentially applicable in batteries for electric vehicles, portable electronics, and stationary energy storage systems. If the technology is successfully scaled, ultrathin lithium anodes could become one of the paths enabling simultaneous reduction of battery pack weight and increase in electric vehicle driving range without a substantial cost increase.

## Fact-Check & Sources

- [Всего 10 микрометров и плотность энергии 504 Вт·ч/кг: Китай приблизился к созданию литиевых аккумуляторов нового поколения](https://www.ixbt.com/news/2026/11/17/vsego-10-mikrometrov-i-plotnost-energii-504-vtckg-kitai-priblizilsia-k-sozdaniiu-litievyx-akkumuliatorov-novogo-pokoleniia.html) - All key figures and technical parameters (anode thicknesses, energy density, number of cycles, coulombic efficiency, role of magnesium, screen-printing method) match the original source text. No discrepancies with the foundation were found.

## FAQ

### What is screen printing in the context of lithium anode production?

It is a method where molten lithium is applied to a copper substrate through a special mask (screen), forming uniform microdisks of specified thickness on the surface. Unlike vapor deposition or impregnation, screen printing allows precise control over lithium thickness and distribution.

### Why are dendrites dangerous for lithium batteries?

Dendrites are thin needle-like lithium crystals that grow during cycling. They can puncture the separator and cause an internal short circuit, leading to capacity degradation, overheating, and in the worst case, fire.

### Are the results ready for mass production?

No. All data obtained are laboratory-scale. Transitioning to industrial production requires solving the challenges of scaling screen printing to large areas and integrating it into existing production lines.

### What energy density was achieved in the experiment?

In the configuration with a nickel-containing cathode and a 20-micrometer anode, the calculated specific energy density was 504 Wh/kg, and the volumetric density was 1071 Wh/L.